What is the definition of a hybrid coating, and what are the performance properties of hybrid coatings?


Selected Answers

From WH Seelinger of State of Kentucky Facilities Management on April 14, 2020:
A hybrid coating has organic and inorganic molecules bonded together on a nano scale to create a morphed particulate.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Coating Materials; EMEA (Europe, Middle East and Africa); Hybrids; Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
SAFE Systems, Inc.

 
Sauereisen, Inc.

 
WEFTEC Show

 
DeFelsko Corporation

 
Tarps manufacturing, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us