How do you repair delaminated areas of an elastomeric polyurea when the majority of the coating system is intact?


Selected Answers

From Aajjay Sunkay of ASSETReifurb Engineerrs on March 20, 2020:
Use a bristle blaster, which is portable power tool equipment or use a grinder to prepare the delaminated area, which also removes loose rust and roughens the exposed metal. Extend the bristle blasting 4 inches beyond the boundary of the delaminated area onto the sound coating and  feather edges all around. Remove the surface dust with dry and clean air. Then apply the coating as per the application procedure suggested by the manufacturer over the delaminated area and extend it 4 inches inches beyond the delaminated area onto the sound coating..

From Janssen Christophe of Lassarat on March 18, 2020:
Remove the damaged area, smoothing the edges with a disc grinder, and then apply the specified primer on the steel or concrete (Surface prep needs to be done before these steps.) Apply an activator on the existing coating around the touch-up and then apply the polyuréa with about 10 inches overlap on the existing coating.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Latin America; Maintenance + Renovation; North America; Polyurea


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
AWWA (American Water Works Association)

 
Fischer Technology Inc.

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Modern Safety Techniques

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us