What generic types of coatings work best as liquid-applied air barriers, considering both cost and effectiveness, and what should be the dry film thickness of this system?


Selected Answers

From yip L C of united chemicals co pte ltd on March 9, 2020:
Two coats of epoxy over concrete will do the trick as air barrier. Taking cost and effectiveness into consideration, the system is 1) a 40% solids, water-based epoxy primer to saturate the concrete porosity with good flow. The thickness will depend on porosity, and  2) a 100 % solids, solventless epoxy primer body coat at 300 microns.

Please sign in to submit your answer this question    

Tagged categories: Air barriers; Asia Pacific; Building Envelope; EMEA (Europe, Middle East and Africa); Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Strand’s Industrial Coatings

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Modern Safety Techniques

 
HoldTight Solutions Inc.

 
CRW

 
Paint BidTracker

 
NLB Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us