How much detail should be included in a specification for the surface preparation and painting of a parking garage exterior that includes tilt-up and structural concrete substrates?


Selected Answers

From Sean Meracle of The Sherwin Williams Company on May 20, 2019:
Aside from cleanliness, ICRI Guideline 310.2R-2013 is an excellent tool for communicating surface preparation expectations, utilizing the Concrete Surface Profile (CSP) comparators.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Latin America; North America; Surface preparation; Surface Preparation


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
Modern Safety Techniques

 
Sauereisen, Inc.

 
AWWA (American Water Works Association)

 
Mitsubishi Gas Chemical America

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us