What is the maximum temperature that an epoxy powder coating can resist when applied on steel substrate?


Selected Answers

From Sukdeb Sil of Birla Carbon India Pvt. Ltd. on March 21, 2019:
300 C

Please sign in to submit your answer this question    

Tagged categories: Coating Materials; Coating Materials; Epoxy


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.

 
DeFelsko Corporation

 
Modern Safety Techniques

 
KTA-Tator, Inc. - Corporate Office

 
Mitsubishi Gas Chemical America

 
Sauereisen, Inc.

 
Fischer Technology Inc.

 
SAFE Systems, Inc.

 
AWWA (American Water Works Association)

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us