Are duplex coatings suitable for immersion service?
Selected Answers
From
norbert ackermann of anticorrosion service on
September 12, 2019:
Duplex coatings - especially TSA with epoxy topcoats - are not recommended for immersion in seawater. There have been numerous failures of duplex coatings on on oil rigs in Scandinavia applied to splash zones and and even to above- waterline areas.
From
Sang Lee of BN Steel Chemical Co.,Ltd. on
December 23, 2018:
Yes