What makes a coating surface-tolerant?


Selected Answers

From Larry Muzia of Exceletech Coating & Applications, LLC on July 30, 2018:
In addition to good wetting, there is also the issue of film stress. Typically, surface tolerant coatings are also formulated to reduce the amount of film stress.

From Erik Andreassen of CPS on July 23, 2018:
Surface-tolerant coatings have excellent wetting properties that are included in the formulation. The provide an excellent solution for epoxy systems that require repairs or upgrading. The wetting properties have the ability to penetrate a suitable prepared substrate in the same way a wood primer works. Most major coating manufacturers have these products in their range.

Please sign in to submit your answer this question    

Tagged categories: Coating Materials; Surface-tolerant coatings


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Modern Safety Techniques

 
Mitsubishi Gas Chemical America

 
SAFE Systems, Inc.

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
AWWA (American Water Works Association)

 
Tarps manufacturing, Inc.

 
DeFelsko Corporation

 
Fischer Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us