Do the balcony floor slabs on the high-rise seaside condo I’m working on in Florida really need cathodic protection?


Selected Answers

From Zenith Czora of Parex Davco on April 17, 2018:
Cathodic protection is designed to halt all the active corrosion of reinforced and pre-stressed concrete slabs and prevent newly installed reinforced concrete slabs from corrosion developing. Penetration of atmospheric contaminants such as CO2 or chlorides to reach the steel bars in the presence of oxygen and moisture will cause the reinforcing steel bars to corrode. Sooner or later, cracking and spalling occur as corrosion products build up around the rebars. In aggressive environments, particularly in coastal areas where chloride contaminants from wind-borne salt spray can be severe, it is therefore very important to provide sufficient cathodic protection to all the rebars of the concrete slab balconies and to other steel structures of the building.

From Michael Halliwell of Thurber Engineering Ltd. on April 16, 2018:
Balconies don't usually have a lot of redundancy to them (especially cantilevered ones). If you have salt water contacting the concrete, you can have chloride-induced deterioration of the concrete itself as well as of the reinforcing steel. Weakened structure with time plus little redundancy plus loading can add up to a failure. I'd say the cathodic protection would be a good idea.

Please sign in to submit your answer this question    

Tagged categories: Cathodic protection; Coatings Technology; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Fischer Technology Inc.

 
WEFTEC Show

 
Tarps manufacturing, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
Sauereisen, Inc.

 
DeFelsko Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us