What is the best way to remove graffiti from the surface of historic stone masonry on a church while preserving the appearance properties of the substrate?


Selected Answers

From Zenith Czora of Parex Davco on December 4, 2017:
Depending on the type of graffiti medium, high pressure washing with hot water or steam cleaning can be used; otherwise, chemical cleaning using alkaline gel or paste-type graffiti remover is preferred because it does not drive the pigment or dyes in the graffiti into the substrates and then can be followed by steam cleaning. Do not use solvent because it will drive  the pigments or dyes in the graffiti medium deeper  into the pores of the substrates.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Building Envelope; EMEA (Europe, Middle East and Africa); Graffiti; Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
SAFE Systems, Inc.

 
Sauereisen, Inc.

 
WEFTEC Show

 
DeFelsko Corporation

 
Tarps manufacturing, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us