What type of material should I use to achieve bright, bold colors that will last on a concrete floor with heavy foot traffic?


Selected Answers

From Jaime Molina of Primary Materials Inc. on June 14, 2017:
A good option would be a metallic epoxy coat. This resin allows the installer to get as artistic with the colors as he or the architect wants. This surface can be topcoated with a good polyurea for an even more durable surface. Durable, artistic and not too expensive.

From Zenith Czora of Master Builders Solutions on June 14, 2017:
You may use tintable, solvent-based acrylic sealer to be tinted to any color of your choice for your first and second coat, then topcoat with polyaspartic clear coating.

From vijay shankar of level floorings on June 13, 2017:
Broadcast dry-shake colored floor hardeners at a dosage of 5 kg per sq m on  green concrete prior to floating and then polish the cured concrete surface to achieve excellent results.

From chris atkins of mott macdonald on June 12, 2017:
Stain the concrete, then use lighting.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Coatings Technology; concrete; Concrete coatings and treatments; Concrete dyes; Concrete floor coatings; Concrete polishing; Concrete stains; Concrete Surfacing; Decorative concrete; EMEA (Europe, Middle East and Africa); Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
GMA Garnet USA

 
Axxiom Manufacturing

 
Abrasives Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us