When coating an aged concrete floor, how should one determine the correct sequence of surface preparation among the options of pressure washing and grinding or other concrete removal and roughening methods?


Selected Answers

From Mika Mack of MAPPA INC. on March 16, 2017:
Determining the onset of concrete failure and deterioration, the strength of the concrete, permeability, pH and RH are all factors, as well as contaminants in the floor . Consult SSPC -SP13 and SSPC-TU 10,  ICRI NO.310.1R and NO. 310.2 and  ACI 546R.

Please sign in to submit your answer this question    

Tagged categories: concrete; Concrete coatings and treatments; Concrete floor coatings; Floor coatings; Floors; Surface Preparation


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
Abrasives Inc.

 
CRW

 
KTA-Tator, Inc. - Corporate Office

 
Seal for Life/STOPAQ

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us