How do you repair polyurea coatings?


Selected Answers

From tom hagen of hagen decorators inc on October 12, 2015:
Typically, the repair would be done with a urethane coating and would require a longer cure time then the polyurea requires.

From Bill downs of VersaFlex on October 12, 2015:
Mechanically abrade the surface area, clean,  and apply a  polyurea repair product available from some polyurea manufacturers.

Please sign in to submit your answer this question    


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Sauereisen, Inc.

 
DeFelsko Corporation

 
Mitsubishi Gas Chemical America

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
Tarps manufacturing, Inc.

 
AWWA (American Water Works Association)

 
Modern Safety Techniques

 
Fischer Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us