What are the most effective procedures for protecting steel and adjacent concrete together?


Selected Answers

From OM PRAKASH JAT of TECH INTERNATIONAL SHARJAH HAMRIAH UAE. on August 18, 2015:
Apply an FBE coating or wrap a viscoelastic coating with outer wrap of PVC or PP.  For exposed locations, the ideal would be wrapping or FBE to avoid continuous damage to a liquid coating. 

Please sign in to submit your answer this question    


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
WEFTEC Show

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us