Which factors are most important in selecting coatings for new concrete?


Selected Answers

From Joe Miller of NextGen Green Building Products, Inc. dba Direct2Contractors.com on January 6, 2016:
The most critical items are 1. the amount of time the installer has to install so the floor is ready when the space must be opened to use; 2. temperatures (surfaces and air) at the time of installation; 3. how the floor coating system looks when its installed; 4. performance after installation and 5.costs. These are the things that I have found to be the concerns of the GC's and the facility owners. If the floor coating system cannot be ready when it's needed, they typically look for some other system solution. Time, after all, is money, as the old adage goes. So fast set times become very critical in the real world.

From Jaime Molina of Primary Materials Inc. on December 22, 2015:
This is a short but very tricky question. The most important factor is obviously 1) the owner’s needs. Here are some pertinent points the contractor should establish with the owner before recommending a coating: a. durability expected of the floor. b. chemical resistance needed. c. abrasion resistance needed. d. slip resistance expected. e. budget. 2) Time: Time restraints will determine if you need to use an efflorescence blocker so you don’t have to wait 28 days. Time to completion will also be an influence. 3) Moisture: What are the moisture vapor emissions? Do you need to apply moisture-stopping epoxy primer? 4) Climate: for obvious reasons.

From Michael Quaranta of OPERATIONS 40 on April 10, 2015:
Hmmm, first would be to typically wait 28 days. Then check the warranty and the MSDS exposure limits of the various coatings. Then  seek out specific applications of coating products where the conditions are like those to be coated. DMA sure covered the requirements! We must not forget to prepare the concrete and test for moisture vapor emissions.

From Stuart Sachs of PRE/view Landscape Architects on April 7, 2015:
The most important factors are use, cost, and surface prep.

From web stokes of DMA on April 6, 2015:
The most important factors are intended use, type and level of traffic, chemical exposure, environmental exposure, impact, and thermal cycling. Desired and required level of texture is important. Other factors might include planned cleaning methods (realistic), desired appearance, moisture vapor content at time of coating,  size and layout of spaces, and turn-around requirements.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Coatings Technology; Concrete coatings and treatments; EMEA (Europe, Middle East and Africa); Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.

 
Seal for Life/STOPAQ

 
Axxiom Manufacturing

 
CRW

 
Sauereisen, Inc.

 
Abrasives Inc.

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us