How can you determine the moisture content of a concrete block (CMU) wall, and how can you judge when the moisture level is low enough to paint?


Selected Answers

From max fleming of fleming coatings on November 4, 2014:
A moisture meter is required. A good moisture meter will have a guide showing when the substrate is dry enough for painting.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Concrete masonry units (CMU); EMEA (Europe, Middle East and Africa); Good Technical Practice; Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Modern Safety Techniques

 
Strand’s Industrial Coatings

 
HoldTight Solutions Inc.

 
NLB Corporation

 
Sauereisen, Inc.

 
Paint BidTracker

 
Tarps manufacturing, Inc.

 
CRW

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us