What are the pros and cons of using shotblasting to remove a coating system from a concrete floor?


Selected Answers

From brent faid of ess resin technologies on September 24, 2014:
Most of the time, if the coating has any millage to it, it doesn't work, but it is great for removing cure and sealers or just old paint.

Please sign in to submit your answer this question    

Tagged categories: Concrete floor coatings; Good Technical Practice; Horizontal shot blasting; Paint and coatings removal; Surface preparation


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.

 
Abrasives Inc.

 
Axxiom Manufacturing

 
Sauereisen, Inc.

 
PaintSquare

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Western Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us