What are the alternatives for removing mildew from uncoated concrete block exteriors before coating?


Selected Answers

From Timothy Knell of Shore Corporation on June 4, 2014:
Depending on your ability to pressure wash and wait for the block to dry, an alkaline cleaner possibly mixed with bleach is a good alternative. If pressure washing is not an option, a formulated hydrogen peroxide cleaner will work best. The slight bubbling action will release the mildew from the pores, and there is little residue from the cleaner that could affect the paint.

Please sign in to submit your answer this question    

Tagged categories: Maintenance + Renovation


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
SAFE Systems, Inc.

 
Sauereisen, Inc.

 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
Fischer Technology Inc.

 
AWWA (American Water Works Association)

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us