What are some ways to improve transfer efficiency of airless spray application?

More items for Coating Application


Selected Answers

From Ken Beauvais of Self on July 28, 2014:
Control the environment in which you are trying to coat.

From Simon Hope of Bilfinger Salamis on September 16, 2013:
Add to this, improvements can be made using air-assisted airless units for actual transfer performance. Also the use of plural pumps on jobs can reduce waste, particularly the heated units as this can improve pot life and quality of finish as well.

From Keith Holdsworth of Eastern Tank on September 12, 2013:
Heated airless spray technology increases transfer efficiency and reduces solvent consumption at the same time.

From Atanas Cholakov of Insignia JFZ on June 17, 2013:
Coatings transfer efficiency varies significantly, depending on  the surface complexity, geometry and size. You may want to consider masking (encapsulating) of the area if it involves field work. Use a skilled spray operator. Refer to the product data sheet of the paint supplier  for information on pump pressure, correct spray tip, etc.

From José Avendaño of Testers y Multimetros 2011 CA on June 17, 2013:
Initially, we must select a right pump rate, gun and nozzle tip. During application, the painter must maintain an adequate distance from the surface, have good application technique (keeping the gun perpendicular to the surface and moving the hand at the correct speed). They should continuously monitor environmental conditions to avoid painting during high winds and excessive temperatures.

Please sign in to submit your answer this question    

Tagged categories: Airless spray; Paint application


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Sidewinder/Persyst Enterprises, Inc.
 
Sidewinder Model M2
 
Load our Refrigeration Machine Distiller Reclaimer with dirty solvent, press the button, you're done. You will have clean gun wash and cleanup solvents, ready for reuse.
 

 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
SABRE Autonomous Solutions
 
Safety
 
Removing blasting operators from harmful environments is our key objective.
 

 
Fischer Technology Inc.
 
Maximize Profits by Monitoring Coating Thickness
 
Learn more by contacting Fischer Technology today: 1.860.683.0781
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
CS Unitec
 
Dust Control Surface Prep Industrial Tools for Steel and Concrete
 
Scarifying • Grinding Scabbling • Descaling Dust collection for safer working conditions. Low-vibration for less worker fatigue. Trelawny™ power tools from CS Unitec. Learn more…
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
ARC / A.W. Chesterton Company
 
Mils Ahead of the Competition
 
Excellent chemical resistance where erosive particulates and thermal cycling conditions may be present.
 

 
Bullard
 
Bullard Made in the USA
 
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us