What type of material should I use to achieve bright, bold colors on a concrete floor that gets heavy foot traffic?


Selected Answers

From Zenith Czora of Durotech Industries, Inc. on August 25, 2021:
if the floor is interior, high solid epoxy self-levelling floor coating with the suitable colourants and the expertise of an applicator in applying the coating is the way to got, otherwise there are also tintable polyspartic clear coating that can be use both ininteror and exterior applications. Slip resistance of the finished coating must be also considered for heavy foot traffic,

From rON Lewis of Corrosion Management Ltd on August 24, 2021:
Timber boards so dirty footwear doesn't touch the concrete.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Color + Design; Concrete floor coatings; EMEA (Europe, Middle East and Africa); Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
Tarps manufacturing, Inc.

 
Abrasives Inc.

 
Sauereisen, Inc.

 
Axxiom Manufacturing

 
CRW

 
KTA-Tator, Inc. - Corporate Office

 
EDCO - Equipment Development Co. Inc.

 
Strand’s Industrial Coatings

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us