What is the best and quickest method for removing a polyurea tank lining?


Selected Answers

From palanisamy moovarsan of TECHNIP on August 14, 2021:
The best and quickest method for removing a polyurea tank lining is ordinary dry abrasive blast and coated.

From Mike Makela of Sunstate Coatings Inc. on August 12, 2021:
UHP blasting 40k

From mauricio gomez of Jifco inc on August 12, 2021:
Removing Elastomeric coatings, and linings my best experience removing that is using a heather torch and scrape with putty knife.

From Dudley Primeaux of Primeaux Associates LLC on August 11, 2021:
If it is an elastomeric polyurea system, that has been properly applied to a properly prepared substrate, the best and fastest method of removal is via High Pressure Water Jetting. And depending upon applied film thickness of the polyurea, may require Ultra-High Pressure Water Jetting.

From Gordon Kuljian of GK Consulting LLC on August 10, 2021:
Hands down UHPWJ with rotating tip and cutting jewels. You will have to deal with the waste-water and waste coating. GK

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Latin America; Maintenance + Renovation; North America; Polyurea; Tank interiors


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
CRW

 
Western Technology Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
Axxiom Manufacturing

 
GMA Garnet USA

 
Abrasives Inc.

 
Sauereisen, Inc.

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us