What is the optimal moisture content for masonry before painting can begin?


Selected Answers

From paarthiban balasubramaniyan of National Basics Company on June 12, 2021:
New concrete must have a moisture content of 4% or less before the coating application commence. Test for retained moisture in concrete as per plastic sheet method ASTM D4263 or by moisture meter or by calcium chloride dome test in ASTM F1869

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Environmental Controls; Latin America; Moisture detection; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
PaintSquare

 
Tarps manufacturing, Inc.

 
CRW

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Western Technology Inc.

 
Abrasives Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us