From Pierpaolo Bonora of TECHNO TRUST on March 31, 2021:
Every time I need to protecty by fire some metal o concrete structures ( Parking, airport, platforms, ..) where in case of fire, the structure must resist a determined time before to collapse or avoid to collaps to give time for fire estiguisher..

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Coating Materials; EMEA (Europe, Middle East and Africa); Intumescent; Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
PaintSquare

 
Axxiom Manufacturing

 
CRW

 
HoldTight Solutions Inc.

 
Abrasives Inc.

 
Western Technology Inc.

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us