New Product Announcement: Eco-Friendly Paint Filler

THURSDAY, AUGUST 3, 2023


Natural mineral filler manufacturer Hoffman Mineral recently introduced a new eco-friendly filler, Sillitin N 75.

According to the company’s release, the product is characterized by its dispersion properties, low yield point, abrasion resistance and matting effect.

“We are very pleased to introduce our new product. With Sillitin N 75, we offer a new filler in the usual best Hoffmann Mineral quality: functional, eco-friendly and made in Germany,” wrote the company.

“In the field of elastomers, Sillitin N 75 is excellently suited for all technical rubber articles and enables a low compression set, a high rebound resilience or a good matting effect.”

Its mineralogical composition reportedly includes 60% neuburg silica, 25% kaolinite, 5% other minerals and 10% amorphous mineral phases.

It can be used for powder and construction coatings, as well as interior dispersion, road marking and facade paints.

   

Tagged categories: Asia Pacific; Coating chemistry; Coating Materials; Coating Materials - Commercial; Coatings Technology; EMEA (Europe, Middle East and Africa); Environmentally friendly; Fillers & surfacers; Green coatings; Hoffman Mineral; Latin America; New Product Spotlight; North America; Silica; Z-Continents