Contractors Needed for GA Storage Tank Rehab

WEDNESDAY, SEPTEMBER 14, 2022


The Brunswick-Glynn County Joint Water and Sewer Commission in Brunswick, Georgia, is currently seeking contractors for the rehabilitation of two 500,000-gallon storage tanks.

Bids are due Oct. 4.

Scope of Work

This project involves rehabilitation and coating of the 500,000-gallon Oglethorpe elevated storage tank (constructed in 2007) and the 500,000-gallon Glynn Place Mall elevated storage tank (constructed in 1987).

Tank interior surfaces will require full abrasive blast-cleaning to Near White (SSPC-SP 10/NACE No. 2) and coating with a zinc-rich primer, polyamidoamine epoxy intermediate and high solids immersion-grade phenalkamine epoxy finish coating.

The owner-approved coating manufacturers are Carboline, Induron and Sherwin-Williams, or an approved equivalent.

Tank exterior surfaces will require solvent cleaning and pressure washing with 3,500 psi water, followed by Power Tool or Brush Off Blast-Cleaning to Bare Metal (SSPC-SP 3, SP 7/NACE No. 4) and coated with a zinc-rich primer, polyamidoamine epoxy first intermediate, and an aliphatic acrylic polyurethane or fluoropolymer second intermediate and topcoat.

The owner-approved coating manufacturers are Carboline, Induron and Sherwin-Williams, or an approved equivalent.

The project includes replacement of foundation sealants with an elastomeric joint sealant. The owner-approved coating manufacturer is Sika, or an approved equivalent.

Containment is required.

Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try PaintBidTracker free!

   

Tagged categories: Bidding; Carboline; contract painting leads; Contractors; Contracts; Government contracts; Induron Coatings; NA; North America; Paint BidTracker; Program/Project Management; Rehabilitation/Repair; Sherwin-Williams; Sika; Tank exteriors; Tank interiors; Tanks; Tanks; Water Tanks

Join the Conversation:

Sign in to our community to add your comments.