CA Construction, Painting Work Out for Bid

FRIDAY, AUGUST 5, 2022


The City of Delano is soliciting bids for the construction of a new park, including an amphitheater, playground equipment and onsite utilities.

The submittal date for this project is Sept. 22.

Scope of Work

This project involves construction and painting of Larry Itliong Unity Park, adjacent to Delano Community Center, in Delano, California.

Exterior work involves a three-coat system of latex on non-traffic concrete, steel, iron and galvanized metal substrates. Three-coat systems of urethane will be required on specified steel, iron, and ferrous metal surfaces and concrete masonry units.

A two-coat system of anti-graffiti coating will be required on concrete seat wall.

Surfaces must be cleaned and prepared in accordance with standards for Solvent Cleaning (SSPC-SP 1), Hand Tool Cleaning (SSPC-SP 2), Power Tool Cleaning (SSPC-SP 3), White Metal Blast Cleaning (SSPC-SP 5/NACE No. 1), Commercial Blast Cleaning (SSPC-SP 6/NACE No. 3), Brush-Off Blast Cleaning (SSPC-SP 7/NACE No. 4), Near White Blast Cleaning (SSPC-SP 10/NACE No. 2), Bare Metal Power Tool Cleaning (SSPC-SP 11), Waterjetting (SSPC-SP 12/NACE No. 5) and Surface Preparation of Concrete (SSPC-SP 13/NACE No. 6).

The manufacturers specified for this project are Benjamin Moore, Coval Molecular Coatings, Dunn-Edwards, Sherwin-Williams and Tnemec.

Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try Paint BidTracker free!

   

Tagged categories: Benjamin Moore; Bidding; Color + Design; Commercial contractors; contract painting leads; Contractors; Contracts; Coval Molecular Coatings; Decorative Finishes; Dunn-Edwards; NA; North America; Paint BidTracker; Painting Contractors; Project Management; Projects - Commercial; Sherwin-Williams; Tnemec; Upcoming projects