FL 2-Tank Coating Project Out for Bid

WEDNESDAY, MAY 13, 2020


The City of Winter Haven is currently seeking contractors to restore and recoat the Lake Lucerne and Elbert Elementary Tanks in Winter Haven, Florida.

Bids are due June 4.

Scope of Work

This project involves restoring and coating the interior and exterior surfaces of existing 300,000-gallon and 250,000-gallon elevated water storage tanks.

Contractors will abrasive blast clean the wet interior surfaces to Near White standards (SSPC-SP 10/NACE No. 2). The interior surfaces will then be coated with a zinc-rich primer and two-coat epoxy system.

The dry interior surfaces will be abrasive blast cleaned to Commercial standards (SSPC-SP 6/NACE No. 3). The interior surfaces will then be coated with a two-coat epoxy system.                                                                  

The exterior surfaces will be abrasive blast cleaned to Commercial standards (SSPC-SP 6/NACE No. 3). The exterior surfaces will then be coated with a zinc-rich primer, epoxy intermediate and polyurethane finish.

The owner-approved coating manufacturers is Tnemec.

A public bid opening will be held immediately following the 2 p.m. deadline via a Zoom meeting. To attend visit: https://zoom.us/j/98148611771.

A site visit can be made by setting up an appointment with Steve Warder at swarder@mywinterhaven.com.

Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try PaintBidTracker free!

   

Tagged categories: Bidding; contract painting leads; Contractors; Contracts; NA; North America; Paint BidTracker; Program/Project Management; Project Management; Tanks; Tanks; Upcoming projects; Water Tanks