Dust-Free Slurry Blaster Debuts

FRIDAY, OCTOBER 23, 2015


Rapid Prep has introduced a new dust-free slurry blaster that the company says is built for a wide variety of blasting and coating needs.

The Greener Blast is a high-performance slurry blasting system that requires a minimum of 375 cfm to a maximum of 1,500 cfm, according to the company. The company also says the slurry blaster is capable of handling drive nozzles ranging from a #6 to a #12 and blasting pressures of 15 psi to 100 psi.

Rapid Prep says the Greener Blast comes with a 50-foot, 1 ¼ inch blast hose; a 50-foot twin line; and a #8 Kennametal XL performance nozzle. It is available for electric or pneumatic power sources.

The Greener Blast is portable and can be either purchased or rented.

More information: www.rapidprep.com.

   