The Paul N. Gardner Company Inc. is offering an ultrasonic pulse echo device designed for use where access is restricted to just one side.

The Pundit PL-200PE can be used to determine concrete slab thickness and find voids, pipes, delaminations, and honeycombing on the subsurface of a substrate, according to the company.

Advanced echo tracking helps identify the main echo and the device has an automatic estimation of pulse velocity, the company says.

The ultrasonic pulse echo is light, ergonomically correct and comes with several accessories and easy-to-use measurement control buttons with optical feedback, according to the company.

More information: gardco.com.

   