Rust-Oleum Wipes Out Surface Prep
Rust-Oleum has introduced industrial-strength wipes designed to speed pre-paint cleaning and other surface preparation tasks.
Rust-Oleum Pre-Paint and Cleaning Wipes are pre-moistened and double-textured: The abrasive side is designed for extra cleaning power: the smooth side, for removing ordinary dirt, dust and grime. The citrus-scented wipes leave no residue, the company says.
The wipes "thoroughly clean the surface to prepare it for optimal coating adhesion," according to Rust-Oleum.
The company notes that paint and coatings can fail prematurely when applied to surfaces with dirt, grease or other contamination.
Rust-Oleum recommends the wipes for use on equipment, machinery, pipes, handrails, walls, doors "or any surface that needs general cleaning or preparation for painting." Each container contains 90 wipes.
More information: www.rustoleum.com/prepaintcleaningwipes.