2 Exterior Insulation Products Debut

THURSDAY, SEPTEMBER 5, 2013


Atlas Roofing Corp. has added two polyisocyanurate exterior wall insulation products for residential and commercial projects to its EnergyShield portfolio.

EnergyShield PRO and EnergyShield PRO2 are suitable for nearly every vertical wall application above grade, including wood frame, steel frame, concrete, CMU, or brick walls, the company’s Atlas Wall CI Board division says.

Pro Products

EnergyShield PRO is a Class-A fire rated, closed-cell polyiso foam core laminated between Class-A durable aluminum facers, according to product literature.

The ASTM C1289 Type I, Class 1 system combines rigid insulation board, high R-value, and water-resistive barrier attributes with an acrylic coated front facer and reflective facer on back, Atlas says.

EnergyShield PRO2 is a Class-A fire rated, ASTM C1289 Type I, Class 2 board, which features an added glass-reinforced polyiso foam core to the EnergyShield PRO, the company says.

For more than 20 years, Atlanta, GA-based Atlas has serviced the building envelope industry with polyiso wall offerings that complement the company’s roof insulation products.

More information: www.atlasroofing.com.

   