A new high-performance elastomeric coating for commercial applications offers a wide-ranging application window that accommodates both low temperatures and high humidity.

Rhino Hybrid 11-50 is a polyurea/polyurethane hybrid elastomeric designed to provide both high tensile strength and good resistance to humidity and substrate moisture during application.

The coating's mix of polyurea and polyurethane chemistries makes it suitable for a wide variety of commercial and industrial applications on structural steel, geotextile, concrete, and wooden structures, the manufacturer says.

Formulation and Features

Rhino Hybrid 11-50 is a 100% solids (zero VOC), high-pressure, spray-applied coating that can be applied in a variety of weather conditions, from hot and dry climates to moderate humidity (up to 85 percent in most instances).

Rhino Hybrid 11-50
Rhino Linings Corp.

Rhino Hybrid 11-50 can be applied in hot, dry climates and in climates up to 85 percent humidity.

The coating's dense chemisty allows it to resist the effects of wind-driven rain, salts and most chemicals, according to Rhino.

Hybrid 11-50 sets within three to five seconds, with 55 shore D hardness, 100 percent elongation, and 2200 psi tensile strength. When used with a Rhino primer, the company says, Hybrid 11-50 will protect steel and concrete from rust, corrosion and degradation.

Hybrid 11-50 is a 1:1 mix ratio, but is also available in a 2:1 mix ratio. Applicators may apply a minimum thickness of 1/16" (62.5 mils/1.5 mm) in a single coat multi-pass application up to 500 ml thick.

Founded in 1988, San Diego-based Rhino supplies polyurethane, polyaspartic and epoxy coatings and linings for industrial, municipal and residential applications.

More information: www.rhinolinings.com.

   

Tagged categories: Coatings Technology; Elastomeric coatings; Hybrids; Industrial Contractors; Paint application; Polyurea; Polyurethane; Protective Coatings; Rhino Linings

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
NLB Corporation

 
HoldTight Solutions Inc.

 
Paint BidTracker

 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
Sauereisen, Inc.

 
CRW

 
Strand’s Industrial Coatings

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us