ITW Polymers Sealants Revamps Units

Thursday, May 30, 2013

Comment | More

ITW Polymers Sealants North America Inc. has reorganized and streamlined its business units to allow for larger-scale operations, the company says.

The ER (Elastomeric Roofing) Systems, Schnee-Morehead, and TACC business units have been combined to form ITW Polymers Sealants North America Inc., based in Irving, TX.

ER Systems provides cool roof coatings technology. Schnee-Morehead is a global provider of sealants for aviation, construction and other industrial sectors. TACC brands include ITW Miracle construction adhesives and ITW Sta'-Put surfacing adhesive.

ERSystems ER Systems
ER Systems

ITW Polymers Sealants North America Inc. includes ER Systems, makers of cool roof technology. The company recently restructured.

The change, effective April 1, was announced May 14.

ITW Polymers Sealants North America Inc. has six facilities operating in Texas, Georgia, Massachusetts, Minnesota, Arizona and California.

ITW Polymers Sealants North America offers expanded sealants solutions to various industries and its key markets, including construction (roofing, surfacing, metal building, and fenestration), aerospace composites and wind energy.

The company's other brands include Acryl-R, Elastek, Pacific Polymers, Permathane, and Tacky Tape.

Illinois Tool Works is a Fortune 200 diversified industrial manufacturer with $18 billion in revenue, operating in mroe than 50 countries worldwide.

   

Tagged categories: Adhesive; Building Envelope; Construction; Cool roof coatings; ITW Polymers Coatings; Roof coatings; Sealant

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
WEFTEC Show

 
Sauereisen, Inc.

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us