Coatings Industry News

Main News Page


New Concrete Fillers Go with the Grain

Thursday, April 25, 2013

Comment | More

Engineers in America's heartland are cooking up a new recipe for the world's most common building material, using post-harvest leftovers from rice, corn and wheat.

Biofuel byproducts are the no-longer-secret ingredient in the mix being developed at Kansas State University, where civil engineers are aiming to increase the strength of concrete while reducing its carbon footprint.

Using the byproducts of biofuels made from corn stover, wheat straw and rice straw, the researchers are hoping to replace some of the portland cement used in making nearly 7 billion cubic meters of concrete each year.

Corn Stover
Iowa State University

Ash from corn stover and other agricultural residue replaced 20 percent of the cement in one concrete sample and made it 32 percent stronger, researchers said.

"Even though making concrete is less energy intensive than making steel or other building materials, we use so much of it that concrete production accounts for between 3 to 8 percent of global carbon dioxide emissions," Kyle Riding, assistant professor of civil engineering, said in a research announcement.

Wood Chips and Wheat Straw

Feraidon Ataie, a doctoral student in civil engineering, is leading the research.

"The idea is to use bioethanol production byproducts to produce a material to use in concrete as a partial replacement of cement," said Ataie.

His team is specifically looking at byproducts from production of cellulosic ethanol, which is biofuel produced from inedible material such as wood chips, wheat straw or other agricultural residue.

Cellulosic ethanol is different from traditional bioethanol, which uses corn and grain to make biofuel. Corn ethanol's byproduct (called distiller's dried grain) can be used as cattle feed, but cellulosic ethanol's byproduct (called high-lignin residue) is often perceived as less valuable.

Strength from Ashes

"With the cellulosic ethanol process, you have leftover material that has lignin and some cellulose in it, but it's not really a feed material anymore," Riding said. "Your choices of how to use it are a lot lower. The most common choices would be to either burn it for electricity or dispose of the ash."

When the researchers added the high-lignin ash byproduct to cement, the ash reacted chemically with the cement to make it stronger. Testing the finished concrete material, the researchers found that replacing 20 percent of the cement with cellulosic material after burning increased the strength of the concrete by 32 percent.

Feraidon Ataie
Kansas State University

"By using these materials we can reduce the carbon footprint of concrete materials," says Feraidon Ataie, whose research has gained funding and attention.

The team has been experimenting with "biofuel pretreatments" to see if they can improve on their ashy mix, Riding said.

From Waste to Asset

Repurposing agricultural waste for use in concrete would be a win-win for both the construction and agricultural industries, researchers say.

Kansas and other agricultural states that produce crops such as wheat and corn could use the straw and stover left after harvesting for making cellulosic ethanol.

"It is predicted that bioethanol production will increase in the future because of sustainability," Ataie said. "As bioethanol production increases, the amount of the byproduct produced also increases. This byproduct can be used in concrete."

Lafarge cement
Myrabella / Wikimedia Commons

Lafarge (pictured) and other companies make cement and aggregates used in 7 billion cubic meters of concrete each year. Concrete production accounts for 3 to 8 percent of global carbon dioxide emissions, Kansas researchers say.

Riding said the development "has the potential to make biofuel manufacture more cost effective by better using all of the resources that are being wasted and getting value from otherwise-wasteful material and leftover materials. It has the potential to improve the strength and durability of concrete. It benefits both industries."

Funding and Publications

Funded in part by a $210,000 grant from the National Science Foundation, the research has included representatives from the University of Texas, North Carolina State University, and the National Renewable Energy Laboratory in Golden, CO.

Some of the work has been published in the American Society of Civil Engineers' Journal of Materials in Civil Engineering.

"If you use this in concrete to increase strength and quality, then you add value to this byproduct rather than just landfilling it," said Ataie. "If you add value to this byproduct, then it is a positive factor for the industry."

   

Tagged categories: American Society of Civil Engineers (ASCE); Building materials; Cement; Coatings Technology; Concrete; Engineers; Green building; Research

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
DeFelsko Corporation

 
NLB Corporation

 
ABKaelin, LLC

 
WEFTEC Show

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
RCG America

 
Norton Sandblasting Equipment

 
Safety Lamp of Houston, Inc.

 
Fischer Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us