Insect-Killing Paint Rolls Out in Africa

Wednesday, April 24, 2013

Comment | More

Malaria-ravaged Ghana has a new weapon to combat the deadly disease: an insecticide paint from Coral Dulux Ghana, an AkzoNobel brand.

The paint was introduced April 17 at a ceremony in the capital city of Accra.

Artilin Vinymat Ultra Paint is manufactured by France-based Artilin and has been approved by European laboratories and government ministries, according to reports.

This video shows how the paint technology works to kill insects.

Malaria, a mosquito-borne disease caused by a parasite, is a leading cause of death and disease in many developing countries. Half of the world’s population lives in areas at risk of malaria transmission across 106 countries and territories, according to the World Health Organization.

The interior coating is non-toxic and safe for human and pets, but contains insecticide and acaricide that is effective at killing flies, mosquitoes, cockroaches, dust mites and termites, as well as eliminating spiders' cobwebs, Coral Dulux said.

How it Works

Artilin Vinymat Ultra Paint, a vinyl aqueous dispersion, features microscopic insecticide crystals firmly bonded into its paint film.

The insecticide crystals release only when an insect lands on the painted surface, the manufacturer says.

The crystals penetrate the legs of the insect and travel to its nervous system, paralyzing and killing the pest in the process, the company reports.

The paint does not release an “offensive smell” and will last for two years, according to reports. It is also mold-resistant, the company says.

‘Major Breakthrough’

“For us, this is a major breakthrough, and we are excited to bring one of the leading paints in the world to the doorstep of our numerous customers,” said Luiz Carlos de Silva, director of Coral Dulux Ghana.

De Silva called the paint "the greatest technological advancement of our time."

mosquito
Alvesgaspar / Wikimedia Commons

Mosquitoes carry parasites that cause malaria, dengue fever and other disease.

The product can be applied by brush or roller like traditional paints; it is available in white and pastel colors, according to information on Artilin’s website.

It can be applied to cement, plaster, wood, cellular concrete and existing matte-finish paint, Artilin said.

Efforts in Other Regions

Other researchers around the world have been working to bring insecticidal properties to paint.

Last year, a Spanish company called Inesba introduced Inesfly, designed to kill mosquitoes and vinchuca, large biting insects that infest thatched roofs and mud walls and carry malaria and Chagas disease.

In February, AkzoNobel officials in India and South Asia told D+D News they were working with the Bill and Melinda Gates Foundation to develop an anti-malaria paint, but were still early in the process. India also has high instances of malaria.

   

Tagged categories: AkzoNobel; Coatings Technology; Coatings technology; Dulux; Interior Wall Coatings; Mold/mildew-resistant coatings; Paint application; Research

Comment from David Hurwitz, (4/24/2013, 6:31 PM)

I am both encouraged by the news of this paint and also cautious about longer term effects. After two years, what happens to the active ingredient crystals? And as with lead containing paints what is the risk of exposure if a human touches the paint as is the issue with small children and lead paint chips! Why are the actives not hazardous to humans? and our pets?


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Abrasives Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
CRW

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
Sauereisen, Inc.

 
Seal for Life/STOPAQ

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us