New Product Announcement: 3D-Printing Resins

Tuesday, November 23, 2021

Comment | More

Sartomer, a business line of global chemicals manufacturer Arkema, recently announced the launch of its new UV-curable resins for 3D-printing and advanced electronic applications.

PRO14729, PRO14730 and PRO14731 are reportedly ultra-low loss materials, capable of providing a dielectric constant (Dk) of ≤ 3.0 and a dissipation factor (Df) of ≤ 0.0032. The resins also have varied viscosities for radio frequency (RF) applications.

“As 3D printing is transforming electronics applications to meet demands of improved performance, functionality and speed to market, we are continuously working to develop materials technologies that optimize electrical performance as well as thermal and mechanical,” said Sumeet Jain, Senior Director of 3D Printing Worldwide at Arkema.

“To meet the growing electronic market’s specific needs, we have invested in a dedicated team of electronics specialists.”

Neal Pfeiffenberger, Technical Business Development Engineer, added, “These new ultra-low dielectric loss materials are part of a growing portfolio of UV-curable solutions for electronics, the first of many innovations in our product range to support this emerging industry.”

According to Sartomer, the resins were designed for use in electronics, antenna elements, radomes, lenses, copper clad laminates, B-staging, server storage and IOT applications.

The company presented the product to the 3D-printing market at Formnext 2021 last week (Nov. 16-19).

   

Tagged categories: 3D printing; 3D Printing; Arkema Inc.; Asia Pacific; Coating Materials; EMEA (Europe, Middle East and Africa); Latin America; New Product Spotlight; North America; Resins; UV coatings; UV curing; Z-Continents

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
EDCO - Equipment Development Co. Inc.

 
Abrasives Inc.

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us