GCP Applied Technologies has recently announced via emailed press release that it has advanced its below-grade waterproofing system for shotcrete foundation.

The advancement arrives, GCP says, in observing the growth of blindside waterproofing in shotcrete applications.

Its product, Preprufe SCS Waterproofing System, is a blindside waterproofing system that is designed for difficult and high-risk tasks of shotcrete applications.

GCP Applied Technologies

GCP Applied Technologies has recently announced via emailed press release that it has advanced its below-grade waterproofing system for shotcrete foundation.

According to GCP, customers will benefit from the waterproofing system through its:

  • Durability designed specifically to withstand the force of shotcrete placement;
  • Post-injected grout fills and seals;
  • Aggressive bond to shotcrete that resists lateral water mitigation; and
  • Resistance to hydrostatic pressure.

   

Tagged categories: Asia Pacific; Below grade waterproofing; Coating Application - Commercial; Coating Materials - Commercial; EMEA (Europe, Middle East and Africa); GCP Applied Technologies; Latin America; New Product Spotlight; North America; shotcrete; Waterproofing; Z-Continents

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
GMA Garnet USA

 
Abrasives Inc.

 
CRW

 
Western Technology Inc.

 
Sauereisen, Inc.

 
Axxiom Manufacturing

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us