The Nebraska Game and Parks Commission in Lincoln, Nebraska, is seeking bids for the upgrade of its cabins.
The submittal date for this project is Jan. 19.
Scope of Work
In this project, all exterior metal shall be coated using a three-coat system made up of one coat of primer followed by two coats of alkyd. Exterior wood surfaces are to be coated using a three-coat system that will consist of one coat of primer followed by two coats of vapex house paint. All concrete and plaster shall be coated using a two-coat system that is exterior latex.
 |
Nebraska Game and Parks Commission |
The Nebraska Game and Parks Commission in Lincoln, Nebraska, is seeking bids for the upgrade of its cabins.
|
All interior masonry will be coated using a three-coat system that is made up of one coat of filler, one undercoat and one coat of alkyd. Interior metal will be coated using a three-coat system that consists of one coat of primer, one undercoat and one coat of semi-gloss enamel.
Interior wood will be coated using a three-coat system composed of one coat of enamel undercoat followed by two coats of semi-gloss enamel. Finally, all concrete on the interior will be coated using a two-coat system that is composed of alkyd.
The brands specified for this project are Pratt & Lambert, PPG, Sherwin-Williams and KWAL.
Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try Paint BidTracker free!
|