Harris County in Houston, Texas, is seeking bids for renovations in the Nuclear Medicine Department at the Lyndon B. Johnson Hospital in Houston.
The submittal date for this project is Dec. 14.
Scope of Work
In this project, all interior ferrous metal surfaces are to be coated using a three-coat system of one coat of primer followed by two coats of acrylic. All nonferrous metal surfaces are to be coated using a three-coat system consisting of one coat of primer followed by two coats of acrylic.
 |
© Google, Inc. 2020 |
Harris County in Houston, Texas, is seeking bids for renovations in the Nuclear Medicine Department at the Lyndon B. Johnson Hospital in Houston.
|
Finally, gypsum board surfaces are to be coated using a three-coat system made up of one coat of primer followed by two coats of latex.
All steel surfaces are to be cleaned using the standards associated with Solvent Cleaning (SSPC-SP 1), Power Tool Cleaning (SSPC-SP 3), and/or Commercial Blast Cleaning (SSPC-SP 6/NACE No. 3).
The brands specified for this project are PPG and Sherwin-Williams.
Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try Paint BidTracker free!
|