ASTM Announces New Test Method for Corrosion

Tuesday, February 5, 2019

Comment | More

Late last month, ASTM International announced a new test method, to be published as D8243, that can help detect corrosion-inducing bacteria in water, which allows for faster remediation and lower costs associated with the damage.

CoffeeandMilk / Getty Images

Late last month, ASTM International announced a new test method, to be published as D8243, that can help detect corrosion-inducing bacteria in water, which allows for faster remediation and lower costs associated with the damage.

According to ASTM International, the enzyme-linked immunosorbent assay is able to detect the sulfate-reducing bacteria.

“Sulfate-reducing bacteria has been identified as a major contributor to microbiologically induced corrosion,” said ASTM International member Alan McQuillin, senior vice president of operations and technology at Modern Water.

For the oil and gas industry, the cost of such corrosion can add up to the $4-30 billion range annually, according to McQuillin.

"The proposed method allows for significantly faster and easier detection of the bacteria versus conventional test methods,” McQuillin said.

   

Tagged categories: AF; AS; Asia Pacific; ASTM; Certifications and standards; Corrosion; EMEA (Europe, Middle East and Africa); EU; Latin America; NA; North America; OC; Quality Control; SA

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Tarps manufacturing, Inc.

 
CRW

 
HoldTight Solutions Inc.

 
Abrasives Inc.

 
PaintSquare

 
Western Technology Inc.

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us