WI Elevated Tank Painting Job Out for Bid

Wednesday, January 9, 2019

Comment | More

The City of Monroe is seeking contractors to paint the Industrial Park Elevated Water Storage Tank in Monroe, Wisconsin. 

Bids are due Jan. 22.

Scope of Work

This project involves coating the interior and exterior surfaces of an existing 500,000-gallon elevated water storage tank.

Contractors will abrasive blast-clean the interior tank surfaces to Near White standards (SSPC-SP10/NACE No..2). The interior wet surfaces will then be coated with a zinc-rich primer and two-coat epoxy system.

City of Monroe

The City of Monroe is seeking contractors to paint the Industrial Park Elevated Water Storage Tank in Monroe, Wisconsin. 

The interior dry surfaces, including the inlet and outlet pipes, will be coated with an epoxy primer and fluid-applied acrylic insulation coating. The interior dry surfaces, including the underside of the tank belly, the access tube, overflow tube, below-grade pipes and valves will be coated with an epoxy primer, fluid-applied acrylic insulation coating and acrylic polymer finish. The interior dry surfaces in need of spot repairs, including ladders and condensate flooring, will be coated with an epoxy primer and finish.

The exterior tank surfaces will be power washed (5,000 psi) and coated with an epoxy spot primer and fluoropolymer spot finish.

The owner-approved coating manufacturer is Tnemec.  

Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try PaintBidTracker free!

   

Tagged categories: Bidding; Contract awards; Government contracts; Jobs; NA; North America; Paint BidTracker; Program/Project Management

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
WEFTEC Show

 
Sauereisen, Inc.

 
Fischer Technology Inc.

 
Tarps manufacturing, Inc.

 
SAFE Systems, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us