Coatings manufacturer Carboline (St. Louis) announced last week the release of a new polyaspartic coating that boasts a quick dry time.

Carboline

Coatings manufacturer Carboline (St. Louis) announced last week the release of a new polyaspartic coating that boasts a quick dry time.

According to the company, Caboquick 200 is a high-build, one-coat, quick-drying polyaspartic that can be applied directly to metal and dry to handle within one to two hours.

The coating is also easy to apply, the company adds, and is ready to spray without thinning.

"In addition to its fast dry to handle time, Carboquick 200 also provides very good color and gloss retention in UV exposure, exceeding the long-term weatherability requirements of SSPC Coating Specification No. 39 Level 3A," said Jeff Anderson, Vice President, Research, Development and Innovation.

According to Carboline, one coat applied DTM at 6-10 mils dry film thickness provides corrosion protection of ISO 12944-6 C 3 High, eliminating the need for a typical primer or intermediate coats, saving time and money.

For more information, visit carboline.com.

   

Tagged categories: Asia Pacific; Carboline; Coatings Technology; DTM (Direct to Metal); EMEA (Europe, Middle East and Africa); Latin America; New Product Spotlight; North America; Polyaspartic

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
Axxiom Manufacturing

 
Tarps manufacturing, Inc.

 
GMA Garnet USA

 
CRW

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us