SSPC Issues AB 3 Revision

Friday, December 15, 2017

Comment | More

SSPC: The Society for Protective Coatings recently announced that it has issued a revision of one of its standards related to abrasive media.

The updates to SSPC-AB 3, Ferrous Metallic Abrasive, involves largely editorial changes, including revisions that incorporate changes to a related standard, SAE J444, Cast Shot and Grit Size Specifications for Peening and Cleaning. AB 3 also now includes a reference to ASTM D7393, Standard Practice for Indicating Oil in Abrasives.

Abrasive blasting
© iStock.com / GlenJ

SSPC has issued a revision of its standard SSPC-AB 3, Ferrous Metallic Abrasive.

SSPC-AB 3 exists to establish requirements for the quality of ferrous-metal abrasives such as iron and steel shot and grit. The standard describes standard shot and grit sizes and shapes, as well as cleanliness, hardness and other properties.

AB 3 is meant to be used as a standard for new abrasive media, not recycled media. It can be used to verify newly purchased media before use. It is one of four abrasive standards offered by SSPC.

The revision was carried out by committee C.2.16, SSPC-AB 3 Revision, chaired by William L. Hansel of CL Coatings.

The newly revised AB 3 can be purchased via the SSPC Marketplace or the SSPC app. 

   

Tagged categories: Abrasive blasting; Abrasives; Asia Pacific; Certifications and standards; EMEA (Europe, Middle East and Africa); Latin America; Maintenance + Renovation; North America; SSPC; Steel Grit; Surface preparation

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
SABRE Autonomous Solutions

 
RCG America

 
SAFE Systems, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Induron Coatings, Inc.

 
DeFelsko Corporation

 
Mitsubishi Gas Chemical America

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us