SSPC: The Society for Protective Coatings is now offering a new standard, issued jointly with the American Association of State Highway Transportation Officials and National Steel Bridge Alliance, on the application of thermal spray coatings to steel bridges.

Steel bridge
© iStock.com / sudok1

SSPC is offering a new standard, issued jointly with AASHTO and National Steel Bridge Alliance, on the application of thermal spray coatings to steel bridges.

SSPC-PA 18/AASHTO-NSBA S.82, developed by committee C.3.19, SSPC/AASHTO/NSBA Thermal Spray Coating Application, complements the existing standard SSPC-CS 23.00/AWS C.2.23/NACE No. 12, Specification for the Application of Thermal Spray Coatings of Aluminum, Zinc, and their Alloys and Composites for the Corrosion Protection of Steel.

The new standard is made to be adopted by transportation departments by reference in their standard specifications. It includes information on pre-production procedures, equipment, materials, surface preparation and application, as well as aspects like repairs and inspection.

The committee was chaired by Jeff Carlson of the National Steel Bridge Alliance.

The new standard is available online via the SSPC Marketplace and on the SSPC app.

   

Tagged categories: AASHTO; Asia Pacific; Bridges; Certifications and standards; Coating Application; EMEA (Europe, Middle East and Africa); Latin America; National Steel Bridge Alliance (NSBA); North America; Paint application; SSPC; Thermal spray; Z-Continents

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
Strategic Materials Inc.

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us