Epoxy Primers Made for Anti-Corrosion

Wednesday, September 27, 2017

Comment | More

AkzoNobel (Amsterdam) has expanded its anti-corrosive primer offerings with Intergard 251HS and Intergard 2575, which are both high-build, low-VOC epoxies.

Intergard 251HS, a zinc phosphate epoxy primer, features extended re-coat suitable for a variety of environments. Intergard 2575, a higher performance zinc phosphate epoxy primer, has the added protection of micaceous iron oxide for corrosive environments.

Both Intergard 251HS and Intergard 2575 share a set of part B converters, which carry color and have two cure speed options. Both coatings require a two-step mixing process, and can be applied as a primer only with a topcoat, or as part of an onsite multi-coat system.

AkzoNobel

AkzoNobel has expanded its anti-corrosive primer offerings with Intergard 251HS and Intergard 2575, which are both high build, low VOC epoxies.

Intergard 251HS is available in red, grey and buff, in a matte gloss, and can be applied with an airless spray, air spray, brush or roller, with a coverage of 401 square feet per gallon. For Intergard 2575, the primer is available in the same colors and gloss, and can be applied using the same tools. The coverage per gallon, however, is 376 square feet.

“We are very proud of this new sustainable and cost-saving epoxy primer range, which builds on International’s record of innovative products that offer tangible results” said Steve Feldman, AkzoNobel’s Protective Coatings Business Director North America.

“Most primers offer good basic protection. But when a primer can provide exceptional protective benefits combined with better compliance and improved productivity, then we’ve just raised the bar on what the industry can expect from their coatings suppliers.”

For more information: http://www.international-pc.com/northamerica.

   

Tagged categories: AkzoNobel; AS; Asia Pacific; Coating Materials; EMEA (Europe, Middle East and Africa); Epoxy; EU; Latin America; NA; New Product Spotlight; North America; Primers; SA

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Sauereisen, Inc.

 
WEFTEC Show

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us