Contractors Sought for 4-Tank Rehab in MD

Friday, August 25, 2017

Comment | More

Saint Mary’s County Metropolitan Commission is seeking contractors for the coating of four existing water tanks located in California, Maryland.

A nonmandatory pre-bid meeting will be held Aug. 30.

Bids are due Sept. 19.

Scope of Work

The project will include rehabilitation of two existing water towers and two hydro-pneumatic tanks.

St. Mary's County water tower
Saint Mary’s County Metropolitan Commission

Saint Mary’s County Metropolitan Commission is seeking contractors for the coating of four existing water tanks located in California, Maryland.

Exterior surfaces of the 150,000-gallon Wildewood tower will be high-pressure cleaned, spot power-tool cleaned to Bare Metal (SSPC-SP 11) where coating failure is present, spot primed and coated with a two-coat acrylic system.

Dry interior surfaces of the Wildewood tower, including baseball piping, will be cleaned to Commercial standards (SSPC-SP 6) and coated with a two-coat epoxy system. The wet interior surface will require abrasive blast-cleaning to Near White (SSPC-SP 10) and coated with a three-coat zinc-epoxy system. The concrete foundation will be pressure-cleaned and receive a two-coat epoxy system.

Contractors will also oversee cleaning and coating of the 250,000-gallon Wilcomico Shores tower. Dry interior surfaces will be cleaned to Commercial standards (SSPC-SP 6) and spot-coated with a two-coat epoxy system. The wet interior will be abrasive blast-cleaned to a Near White finish (SSPC-SP 10) and coated with a three-coat zinc-epoxy system.

Wilcomico Shores tower exterior surfaces will be abrasive blast-cleaned to Commercial standards (SSPC-SP 6) and coated with a four-coat zinc-epoxy-polyurethane-fluoropolymer system. The concrete foundation surfaces will be pressure cleaned and coated with a two-coat epoxy system.

The exterior of both 8,000-gallon hydro-pneumatic tanks will be cleaned to Commercial standards (SSPC-SP 6) and coated with a four-coat zinc-epoxy-polyurethane-fluoropolymer system. Wet interior surfaces of both tanks will require cleaning to a Near White finish (SSPC-SP 10) and coating with a three-coat zinc-epoxy system.

The existing coatings on three of these tanks currently contain lead, chromium and cadmium. Containment is required.

Reported by Paint BidTracker, a construction reporting service devoted to identifying contracting opportunities for the coatings community. Try PaintBidTracker free!

   

Tagged categories: Contract awards; contract painting leads; Contracts; Government contracts; Jobs; NA; North America; Paint BidTracker; potable water; Program/Project Management; Water Tanks

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
EDCO - Equipment Development Co. Inc.

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
HoldTight Solutions Inc.

 
Abrasives Inc.

 
CRW

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Strand’s Industrial Coatings

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us