Tuesday, August 8, 2017

Comment | More

Singularity Black is the world’s new blackest black coating, and this time, it will be available for all artists to use.

NanoLab Inc., a carbon nanotube manufacturer based out of Waltham, Massachusetts, has produced a contender in the competition for the world’s blackest black—Singularity Black. The coating, which is a carbon nanotube paint, is open for anyone and everyone to use—even artist Anish Kapoor, who has the exclusive artistic use of Surrey Nanosystems' Vantablack (the original blackest black).

The artistic world has not stopped reacting to Vantablack's exclusivity, most noteably artist Stuart Semple, who has created several pigments over the past few years and has "banned" Kapoor from using them.

Jason Chase

Jason Chase, an artist also based out of Massachusetts, used Singularity Black to cover a cast-iron gummy bear, displaying the piece against a wooden circle painted with rainbow colors to offset the blackness of the material.

Jason Chase, an artist also based out of Massachusetts, says that it's important for all artists to have access of new paints and pigments.

“Artists are always the ones who take new materials and push them to new limits,” he said in a statement.

Chase is the first artist to use the new Singularity Black by covering a cast-iron gummy bear and displaying the piece against a wooden circle painted with rainbow colors to offset the darkness of the material. Known as Black Iron Ursa, the piece gives the contrast between the absence of light and the rainbow, with the gummy bear itself appearing flat and featureless.

Vantablack vs. Singularity Black

Despite the moniker of the “world’s blackest black,” Vantablack is not, in fact, a paint. Instead, the coating is a dense network of carbon nanotubes, which are grown in a high-heat chamber. Surrey NanoSystems—the company that created Vantablack—has since gone on to create a spray paint version of Vantablack.

Singularity Black, on the other hand, combines carbon nanotubes with a binding agent serving as a stabilizer. The coating was created under contract for NASA in 2011, and was a completely separate venture from Surrey's Vantablack. NanoLab’s coating is used by the space agency for the observation of faraway stars, by coating the equipment with it in order to absorb stray light that might interfere with sensors.

According to NanoLab Systems, Singularity Black should be applied in a spray booth or fume hood, onto a metal surface. A Badger 150 airbrush is most suitable for small scale applications.

After the coating has been applied, a temperature of 572 degrees Fahrenheit is required to activate the coating, along with eliminating the binder, which leaves the carbon nanotubes in a porous arrangement for maximum light absorption. Once this has happened, it becomes a “no-touch” surface. NanoLab also offers a tougher version that can handle incidental contact, but the coating can be repaired with a brush and a heat gun.

Singularity Black passes 400 cleanliness specifications per the Institute of Environmental Sciences and Technology, while also passing thermal cycling tests in a range of 140 degrees and 185 degrees Fahrenheit. Singularity Black also passes NASA General Environmental Verification Specification, along with the Delta IV rocket vibration tests.

The primary downside to Singularity Black is its fragility.

“If you touch it, it’s going to flake off, kind of like when you touch a butterfly’s wings,” Chase told the Boston Globe.

Future Plans

Currently, Chase plans to share his research on how to make the most out of Singularity Black in an artistic sense, with hopes of curating a show featuring works made with the new coating.

NanoLab also estimates that Singularity Black will cost in the low- to mid- hundreds range for 250 milliliters to one liter of paint.

Black Iron Ursa will be on view Aug. 24 at Laconia Gallery, in Boston, and Sept. 6 at the Artisan’s Asylum in Somerville, Massachusetts.

   

Tagged categories: Asia Pacific; carbon nanotubes; Coatings; Coatings technology; Color + Design; Color + Design; EMEA (Europe, Middle East and Africa); Latin America; North America

Comment from peter gibson, (8/8/2017, 10:35 AM)

What next..I thought we had black. I've been duped.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
CRW

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us