Polymer Emulsion Made for DTM Coatings

Thursday, June 15, 2017

Comment | More

Coating manufacturer Michelman (Cincinnati, Ohio) recently introduced ProHere A 03010, a new waterborne, low-VOC polymer emulsion for direct-to-metal coatings.

According to the company, ProHere A 03010 is a waterborne acrylic polymer emulsion that resists corrosion, and provides gloss as well as optical clarity. The new product can be used in formulating a single-layer, DTM coating, or a topcoat or primer in multi-coat systems. The emulsion also provides water resistance, as well as hardness, according to Michelman, and the company sees it as a component for feasible waterborne alternatives to more traditional solvent-borne DTM coatings.

Michelman

ProHere A 03010 is a waterborne acrylic polymer emulsion that resists corrosion, and provides gloss as well as optical clarity, according to manufacturer Michelman.

The emulsion has a typical pH of eight to nine, with a minimum film-forming temperature of 86 degrees Fahrenheit, and is 49-51 percent non-volatile.

According to Michelman, the company's ProHere emulsions contain both polymer resins that can serve as organic binders, as well as lubricants and anti-scratch additives for metal processing and in-use lubricants.

“Waterborne coating systems continue to gain in popularity and acceptance. However, there are still many coatings market segments that are lacking in effective and low emission polymeric binder and surface additive options,” says Julien Verron, industry manager of Coatings Group at Michelman.

Michelman's ProHere line includes emulsions and dispersions for metal coatings.

For more information, go to http://www.michelman.com/.

   

Tagged categories: Coatings raw materials manufacturers; DTM (Direct to Metal); Polymers; Raw materials

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
International Paint/AkzoNobel
 
Chartek 2218
 
Chartek 2218 is an epoxy PFP system for UL1709 installations offering one coat rapid cure application enabling improved production rates & reduce overall costs.
 

 
HoldTight Solutions Inc.
 
Clean surfaces simply don't rust, and no other product cleans like HoldTight®
 
HoldTight® is a wet blasting additive that decreases the water’s surface tension, allowing it to get into the pores of the surface and remove ALL contamination, including salts, acids, abrasives, light oils, and greases. HoldTight® leaves behind zero unwanted residue, and evaporates with the water, providing a surface that is thoroughly clean and ready for a tightly adhered coating bond for up to 72 hours.
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
US Minerals
 
Hit Harder. Clean Faster.
 
Learn more at www.blackdiamondabrasives.com.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us