British Steel has announced that 200-meter lengths of its corrosion-resistant Zinoco rail have been put into service as part of a Network Rail project in Scotland in what the company calls the first example of ultra-long corrosion-resistant rail in use.

British Steel, a spinoff of Tata Steel formed in 2016, introduced Zinoco last summer, having developed the product at the request of Network Rail, the agency responsible for the U.K’s rail lines. Zinoco (which stands for “Zinc No Corrosion”) is made by covering the steel rail with a zinc oxide coating.

Zinoco
British Steel

British Steel delivered 216-meter (709-foot) lengths of Zinoco corrosion-resistant rail for installation in the Inverkeithing Tunnel, near Edinburgh.

The zinc oxide, the company explains, offers both barrier protection and corrosion protection in the form of a sacrificial anode. Testing at British Steel’s Scunthorpe headquarters showed that the new rail line can be expected to outlast traditional uncoated rail by around five times in a variety of aggressive environments, according to the company.

Zinoco in Use

In November, the company supplied 108-meter (354-foot) lengths of the rail to Network Rail for a project in the Patchway Tunnels, between Cardiff and Bristol.

The newest project involves 216-meter (709-foot) lengths delivered for installation in the Inverkeithing Tunnel, near Edinburgh. British Steel says the use of the ultra-long corrosion-resistant rail pieces helped eliminate some 50 welds that would have been necessary to make on site using more traditional materials.

Network Rail has said that about 96 percent of its steel is made at the Scunthorpe facility—previously under the Tata name—and now as British Steel. The agency signed a contract with the company in 2016 for the delivery of about 288 million pounds’ worth of steel through 2019.

   

Tagged categories: Barrier coatings; Coating Materials; Europe; Rail; Sacrificial coatings; Steel; Zinc anodes; Zinc oxide

Comment from Mario Colica, (6/8/2017, 11:22 AM)

This's another example of the efficiency of Zn Thermal spray process; Technology that is on the top of the remedies to prevent or contrast rust of steel


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
SAFE Systems, Inc.

 
Fischer Technology Inc.

 
AWWA (American Water Works Association)

 
Tarps manufacturing, Inc.

 
Mitsubishi Gas Chemical America

 
DeFelsko Corporation

 
Sauereisen, Inc.

 
Modern Safety Techniques

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us