Friday, February 10, 2017

Comment | More

A Polish rail vehicle manufacturer is reportedly working with a coating manufacturer from Berlin to test the world’s first biobased railcar coating.

Train with biobased coating
Covestro

Polish railcar manufacturer Newag SA has coated two diesel locomotives with a biobased paint made by Lankwitzer Lackfabrik.

Newag SA has coated two diesel locomotives with a paint made by Lankwitzer Lackfabrik, formulated in part with Desmodur eco N 7300, a plant-based hardener developed by raw materials supplier Covestro. Lankwitzer’s EVOClear 294 / PH 94-0000 was applied like a standard clearcoat, and according to the manufacturer, performed as well as a more traditional polyurethane under testing.

Plant-Based Hardener

Covestro’s Desmodur eco N 7300 was first released in 2015; the pentamethylene diisocynate-based material is made from field corn that’s not suitable for human consumption. It was described as being on par with conventional, petrochemical-based hardeners in terms of properties like hardness and resistance to weathering, scratching and chemicals.

The hardener was named Bio-Based Material of the Year 2015 at the International Conference on Bio-Based Materials that year.

Other details of the coating formulation were not immediately available from Lankwitzer.

Added Value

Covestro, which participated in the development of the coating, says the new clearcoat from Lankwitzer stands up to chemicals used in graffiti removal, an important attribute for railcar coatings.

“With a new product, a coating manufacturer’s first priority is, of course, to fulfill the customer’s specifications,” said Mateusz Fedko, project manager at Newag. “If the coating offers added value on top of that, as is the case here with the renewable raw materials, it gives us a very good opportunity to set ourselves apart from the competition.”

Eying Other Applications

Lankwitzer is reportedly looking to expand the use of the new product into other applications.

“I am certain this biobased clearcoat will also create value for our customers in other industries,” said Lankwitzer’s Michael Voxbrunner.

   

Tagged categories: Asia Pacific; Bio-based materials; Coating chemistry; Coating Materials; Coatings Technology; Covestro; EMEA (Europe, Middle East and Africa); Green coatings; Hardeners; Latin America; North America; Railcars

Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
CRW

 
Sauereisen, Inc.

 
Abrasives Inc.

 
Seal for Life/STOPAQ

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us