New research from an international team suggests that, while cement production is a major generator of carbon dioxide gas, concrete and other cement-based materials also absorb a considerable amount of CO2 throughout their lifetime.

The new study comes via the University of California, Irvine, where physicist Zhu Liu and Steven Davis, an associate professor of Earth system science, have been working with an international, multi-institution team of scientists to study carbon emissions and cement. The team’s main finding: Cement seems to actually act as a “carbon sink,” absorbing CO2 so it cannot contribute to the greenhouse effect.

Concrete
Steven Davis /  UCI

Though its production does create carbon dioxide gas, cement seems to actually act as a “carbon sink,” absorbing CO2 so it cannot contribute to the greenhouse effect.

“It sounds counterintuitive, but it’s true,” Davis said. “The cement poured around the world since 1930 has taken up a substantial portion of the CO2 released when it was initially produced.”

Taking in CO2

It happens through a process called carbonation: Cement materials like concrete and mortar actually absorb CO2 through their pores, removing the gas from the air and preventing it from trapping heat within Earth’s atmosphere.

The researchers aren’t saying a concrete cityscape is just as good as a forest for bringing down carbon in the atmosphere—cement production is still responsible for a net increase in CO2. But perhaps it’s not quite the heavy polluter some had previously thought.

Production and Absorption

According to the study, cement production released 38.2 gigatons of CO2 into Earth’s atmosphere during the period between 1930 and 2013, both from limestone conversion and from fossil fuels burned in the production process. But the researchers estimate that cement absorbed 4.5 gigatons of CO2 through carbonation during that same period.

Cement plant
© iStock.com / tupungato

Cement production releases CO2 into the atmosphere both as a direct result of limestone conversion and from fossil fuels burned in the production process.

That’s nearly 12 percent of all CO2 produced during cement production—and, the study notes, it’s about 43 percent of the CO2 created by limestone conversion, which is a necessary step in cement production. The conclusion it all points to: It’s fossil fuels, not cement production itself, that contribute most heavily to CO2 emissions and the resulting climate effects.

“Cement has gotten a lot of attention for its sizable contribution to global climate change, but this research reinforces that the leading culprit continues to be fossil fuel burning,” Davis said.

International Project

The study, titled “Substantial Global Carbon Uptake by Cement Carbonation,” was published last month online by Nature Geoscience. In addition to Davis, it was authored by 18 other scientists representing a total of 17 institutions in China, Denmark, France, South Korea, Spain, the U.K. and the United States.

   

Tagged categories: Asia Pacific; Carbon footprint; Cement; Coating Materials; Colleges and Universities; concrete; EMEA (Europe, Middle East and Africa); Emissions; Environmental Protection; Greenhouse gas; Latin America; North America; Research

Comment from chris atkins, (12/19/2016, 4:42 AM)

Ignoring the CO2 produced in the energy required to make cement, when you make cement, you drive of CO2. When concrete carbonates it absorbs it, but carbonation is a slow process and rarely penetrates to a significant depth. I don't see how it can ever be carbon neutral. 43% of the carbon dioxide produced by conversion of limestone has been estimated as the figure reabsorbed. Still means 57% hasn't and ignores the energy required in the production of cement.


Comment Join the Conversation:

Sign in to our community to add your comments.


Advertisements
 
Sauereisen, Inc.

 
Modern Safety Techniques

 
ABKaelin, LLC

 
NLB Corporation

 
Fischer Technology Inc.

 
Induron Coatings, Inc.

 
RCG America

 
WEFTEC Show

 
Sidewinder/Persyst Enterprises, Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us